Detailed poster information
| Poster title | Degradation of Inconel 617 and Inconel HX in high-temperature helium environments (900 °C, 101 kPa). |
|---|---|
| Poster code | WP 03.02 |
| Authors | |
| Form of presentation | Poster |
| Topics |
|